Logo
  • Resources
    • COTS for Space WEBINARS
    • ACCEDE 2022 Workshop on COTS
    • EEE COMPONENTS
    • SPECIFICATIONS / QPLs
    • EVENTS / WEBINARS
    • SPACE TALKS
    • TECH ARTICLES
    • MANUFACTURERS NOTIFICATIONS
  • Laboratory Services
    • LABORATORY STANDARD TESTING
    • NON STANDARD TESTING
    • SILICON CARBIDE -SiC- DIODES
    • CROWDTESTING
    • OPTOELECTRONICS
    • SMALL SATS
    • REPRESENTATIVE PROJECTS / PAPERS
  • Additional Services
    • INDUSTRY 4.0 CYBERSECURITY (IEC 62443)
    • PENETRATION TEST
    • CYBERSECURITY CERTIFIED (CSC)
    • CODE SCORE MATRIX
    • LONG-TERM STORAGE OF WAFERS
    • ELECTRONIC DESIGN
  • Tools
    • COMPARATOR
    • MY DCLs/BOMs
    • STOCKPLACE
  • About Us
  • My Request
  • Sign In
  • Resources
    • COTS for Space WEBINARS
    • ACCEDE 2022 Workshop on COTS
    • EEE COMPONENTS
    • SPECIFICATIONS / QPLs
    • EVENTS / WEBINARS
    • SPACE TALKS
    • TECH ARTICLES
    • MANUFACTURERS NOTIFICATIONS
  • Laboratory Services
    • LABORATORY STANDARD TESTING
    • NON STANDARD TESTING
    • SILICON CARBIDE -SiC- DIODES
    • CROWDTESTING
    • OPTOELECTRONICS
    • SMALL SATS
    • REPRESENTATIVE PROJECTS / PAPERS
  • Additional Services
    • INDUSTRY 4.0 CYBERSECURITY (IEC 62443)
    • PENETRATION TEST
    • CYBERSECURITY CERTIFIED (CSC)
    • CODE SCORE MATRIX
    • LONG-TERM STORAGE OF WAFERS
    • ELECTRONIC DESIGN
  • Tools
    • COMPARATOR
    • MY DCLs/BOMs
    • STOCKPLACE
  • About Us
  • My Request
  • Sign In
Assembly Processes, Packaging and Assembly

Stud Bumping

  • Posted by doEEEt Media Group
  • On March 16, 2020
  • 0

Alter Technology UK, has the ability to Gold (Au) stud bump wafers and individual die making them ready for a subsequent flip chip attach process

Gold stud bumping forms Au bumps using a process similar to Au ball wire bonding. Like wire bonding, it forms an Au ball (stud). However, the wire is terminated after the first bond so there is only a bump on the die.

Au stud bumping requires no Under Bump Metalization (UBM) or special wafer preparation, unlike the requirements for solder bumping. It also offers finer bump spacing than most solder bump technology without the added expense of a solder re-distribution layer.

Au stud bumps can be used on individual die or wafers and typically have much lower set-up costs than a solder bump approach. The ability to bump individual die makes Au stud bumping an extremely valuable tool in the prototyping phase and a viable option for volume manufacturing.

For many sensitive devices such as lasers, MEMS, and sensors, the use of flux or adhesives is not allowed, and a thermosonic or thermocompression Au-Au attach process offers a reliable flux-free process to improve the device reliability.

Stud Bumping

Depending on the application, Au stud bumps can be produced in various diameters and shapes. For example, Stud bumps with diameters of 40-100um can be produced with heights of 20-80um. Co-planarity of +/-2.5um can be achieved without the coining process. Stacked bumps can increase the stand-off distance between the die and substrate to help accommodate substrate thickness variations and minimize CTE differentials. Gold stud bumps with pointed tips can be used for subsequent epoxy dipping.

Alter Technology UK’s expertise and capability in Gold Stud bumping will reduce risk and time to market for your Gold stud bumping requirements and provide a cost-effective manufacturing option.

Contact us for more information

  • Author
  • Recent Posts
doEEEt Media Group
doEEEt Media Group
doEEEt media is the group behind every post on this blog.
A team of experts that brings you the latest and most important news about the EEE Part and Space market.
doEEEt Media Group
Latest posts by doEEEt Media Group (see all)
  • Miniature RF Connectors - April 29, 2025
  • Miniature RF Connectors for high-performance testing - April 24, 2025
  • Space-Grade components available for immediate delivery - April 10, 2025

Previous Post

Wire Bonding Services

Next Post

Encapsulation and Hermetic sealing
0 comments on Stud Bumping
Recent Posts
  • Miniature RF Connectors
  • Miniature RF Connectors for high-performance testing
  • Space-Grade components available for immediate delivery
  • Introduction to RD ALFA Microelectronics: Components and Capabilities
  • Managing EEE components for LEO and lower cost space missions
Scroll

doEEEt.com

DoEEEt: Electrical Electronic Electromechanical (EEE) parts database. Find (EEE) components/parts products and datasheets from hundreds of manufacturers.

Privacy Policy and Legal Notice

Copyright

Cookie Policy

Copyright © 2021 ALTER TECHNOLOGY TÜV NORD S.A.U

Company

About us

Contact us

How does doEEEt works? – FAQ

ALTER Laboratory Services

Microwave and RF Testing

Small Sats Testing

COTS components Testing

Authenticity Test